03-26-2018, 03:49 AM
8011A-H14 aluminum is a type of 8011A aluminum. It is furnished in the H14 temper. To achieve this temper, the metal is strain hardened to a strength that is roughly halfway between annealed (O) and full-hard (H18). The graph bars on the material properties cards below compare 8011A-H14 aluminum to: otherwise unclassified aluminums (top), all aluminum alloys (middle), and the entire database (bottom). The length of each bar shows the given value as a % of the largest value in the relevant set.